Item |
Time |
Temp |
Pressure |
Tips/comments |
Ceramic | 180C | 180 sec | Medium-High | |
Metal sheets | 190C | 100 sec | High | face down, remove protective film |
Polyester | 180C | 50-60 sec | Light - Medium | |
Coated MDF | 185C | 50-60 sec | Light - Medium | remove protective film |
Rock slate |
190C | 420 sec | Hight | face down, pre-heat the back of the slate for 120 sec |
|
||||
|